Microstructure of POPbeton



Fly ash as raw material, polished specimen.

Detail of a polished specimen.

Aggregate interface.

Reinforcement interface.

POPbeton after 2 years of placement in a Na2SO4 solution.

POPbeton after 7 years of placement in sea water.

POPbeton (mortar) after 3 months of placement in H2SO4.

Fired POPbeton (specimens from right): firing temperatures of 20°C, 600 °C, 800°C and 1000 °C , both orange pieces were fired to 1000°C.